Effect Of Water-Cement Ratio On Performance Of Seaweed-Modified Mortars
Figure 4: [Adhesion strengths of preparation 1 with 27% cement and preparation 2 with 26% cement, where ♦- 28 days in normal climate, ■-21 days in normal climate, 7 days in water, ▲- Calcium hydroxide, 28 days at normal climate and ●- preparation 2 normal climate.]
![[Adhesion strengths of preparation 1 with 27% cement and preparation 2 with 26% cement, where ♦- 28 days in normal climate, ■-21 days in normal climate, 7 days in water, ▲- Calcium hydroxide, 28 days at normal climate and ●- preparation 2 normal climate.]](https://www.europeanproceedings.com/files/data/article/94/5435/AIMC2018120.fig.004.jpg)