Figure 2: [Flexural strengths for preparation 1 with 27% cement and preparation 2 with 26% cement, where ♦- 28 days in normal climate, ■-21 days in normal climate, 7 days in water, ▲- Calcium hydroxide, 28 days at normal climate and ●- preparation 2 normal climate.]

 [Flexural strengths for preparation 1 with 27% cement and preparation 2 with 26% cement, where ♦- 28 days in normal climate, ■-21 days in normal climate, 7 days in water, ▲- Calcium hydroxide, 28 days at normal climate and ●- preparation 2 normal climate.]